  1. 61. Potassium sulfate (2%) added to dental stone acts primarily to:

    • A. Retard setting and increase strength
    • B. Accelerate setting and reduce setting expansion
    • C. Increase hygroscopic expansion
    • D. Reduce the water/powder ratio required
    Show answer & explanation

    Answer: B. Accelerate setting and reduce setting expansion

    Potassium sulfate is the classic chemical accelerator for gypsum products. It increases the solubility of the hemihydrate, so dihydrate crystals nucleate and precipitate faster, shortening setting time. At the same time it reduces setting expansion, because the more rapid, numerous nucleation produces smaller, less divergent crystals that exert less outward thrust. For this reason potassium sulfate (often combined with borax to restore working time) forms the basis of 'anti-expansion solutions' used in model and die stones. It does not retard setting (borax and citrates do that), it does not change the water/powder ratio (that depends on hemihydrate crystal form - alpha vs beta), and hygroscopic expansion depends on adding water during setting, not on chemical modifiers. High-yield point: accelerators and retarders generally both reduce setting expansion.
    Discuss this question
  2. 62. Hygroscopic setting expansion of gypsum exceeds normal setting expansion mainly because:

    • A. Extra hemihydrate dissolves in the added water
    • B. Crystal growth is not restrained by the surface tension of the water film
    • C. The dihydrate crystals become larger due to slower nucleation
    • D. Added water reacts chemically to form additional dihydrate
    Show answer & explanation

    Answer: B. Crystal growth is not restrained by the surface tension of the water film

    When gypsum sets in air, water is consumed by the hydration reaction and the remaining water between crystals forms thin films whose surface tension pulls the growing crystals together, restraining their outward growth. If water is added during the setting process (immersion or water added to the investment ring liner), the water consumed is continuously replaced, so the crystals are surrounded by free water and grow outward without this surface-tension restraint. The result is a hygroscopic expansion that may be about twice (or more) the normal setting expansion. It is a physical phenomenon, not extra chemical reaction or additional hemihydrate dissolution. Hygroscopic expansion is exploited in gypsum-bonded investments for compensating casting shrinkage of gold alloys; it increases with finer silica, higher silica content, earlier immersion and lower W/P ratio.
    Discuss this question
  3. 63. Type V (high-strength, high-expansion) die stone is preferred over Type IV for some castings because it:

    • A. Has better surface hardness due to a higher W/P ratio
    • B. Shows no setting expansion and better accuracy
    • C. Is made of beta-hemihydrate, giving greater strength
    • D. Has greater setting expansion to compensate for larger alloy solidification shrinkage
    Show answer & explanation

    Answer: D. Has greater setting expansion to compensate for larger alloy solidification shrinkage

    ISO/ADA classify gypsum into five types. Type IV (high-strength, low-expansion) has setting expansion of about 0.00-0.10%, while Type V (high-strength, high-expansion) has 0.10-0.30% and also the highest compressive strength (about 48 MPa vs 35 MPa). Base metal alloys and some newer alloys have greater solidification shrinkage than traditional high-gold alloys, and the extra expansion of Type V dies helps compensate for this, producing a die slightly larger than the prepared tooth. Both Types IV and V are made from alpha-hemihydrate (densite), whose dense prismatic particles require less mixing water (W/P about 0.19-0.24). A lower W/P - not a higher one - produces higher strength and surface hardness. Beta-hemihydrate (plaster of Paris) is porous, irregular, needs more water and gives weaker products.
    Discuss this question
  4. 64. A stone die poured 5 minutes after taking an addition silicone impression shows multiple small surface voids. The most likely cause is:

    • A. Sulfur contamination from latex gloves
    • B. Release of hydrogen gas from the impression
    • C. Release of ethanol by-product
    • D. Imbibition of water by the impression
    Show answer & explanation

    Answer: B. Release of hydrogen gas from the impression

    Addition silicone (polyvinyl siloxane) sets by a platinum-catalysed hydrosilation reaction between vinyl-terminated siloxane and silane (Si-H) groups. There is no reaction by-product, which is why the material has excellent dimensional stability. However, if residual Si-H groups or moisture are present, a secondary reaction can release hydrogen gas from the set impression for some time after setting. If gypsum is poured too early, the evolved hydrogen produces pinpoint voids on the die surface. Remedies are to delay pouring (classically 1-2 hours) or to use products containing hydrogen scavengers such as finely divided palladium, which can be poured immediately. Ethanol release and shrinkage are features of condensation silicone; water as by-product is from polysulfide; imbibition is a problem of polyether and hydrocolloids. Latex sulfur contamination causes inhibition of setting (tacky surface), not voids in the die.
    Discuss this question
  5. 65. The modulus of resilience of an orthodontic wire is:

    • A. Directly proportional to elastic modulus
    • B. The total area under the stress-strain curve
    • C. Equal to ultimate tensile strength divided by elastic modulus
    • D. Proportional to the square of proportional limit divided by twice the elastic modulus
    Show answer & explanation

    Answer: D. Proportional to the square of proportional limit divided by twice the elastic modulus

    Resilience is the amount of energy per unit volume a material can absorb without permanent deformation, i.e. the area under the elastic (linear) portion of the stress-strain curve up to the proportional limit. Mathematically, modulus of resilience = PL squared / 2E, where PL is the proportional limit and E is the elastic modulus. Therefore a wire with high proportional limit and LOW elastic modulus stores more energy and delivers it over a longer range, which is clinically desirable for orthodontic wires (e.g. beta-titanium and NiTi compared with stainless steel). Toughness, by contrast, is the total area under the stress-strain curve up to fracture, including the plastic region. The ratio of strength to modulus (PL/E) relates to springback or flexibility, not resilience. This formula is a frequently tested numerical concept in entrance exams.
    Discuss this question
  6. 66. Which elastomeric impression material shows the highest elastic recovery (least permanent deformation) after removal from undercuts?

    • A. Addition silicone
    • B. Polysulfide
    • C. Condensation silicone
    • D. Polyether
    Show answer & explanation

    Answer: A. Addition silicone

    Elastic recovery is tested by compressing the set material (e.g. 12% strain for 30 s) and measuring residual deformation. Addition silicone (PVS) shows the best recovery, about 99.5-99.9% (permanent deformation roughly 0.05-0.4%), because its highly cross-linked network formed by addition polymerization is very elastic. Polyether follows closely (about 98.5-99%), condensation silicone around 98.5-99.5%, while polysulfide is the poorest (about 96-97%) owing to its more viscoelastic, less cross-linked structure, which is why polysulfide impressions should be removed with a quick snap and poured within an hour. Clinically, a material with high elastic recovery tolerates deeper undercuts and delayed or multiple pours. Addition silicone also has the best dimensional stability because no by-product is lost, making it the material of choice when pouring may be delayed.
    Discuss this question
  7. 67. In irreversible hydrocolloid (alginate), the component that controls working time is:

    • A. Calcium sulfate dihydrate
    • B. Trisodium phosphate
    • C. Potassium alginate
    • D. Diatomaceous earth
    Show answer & explanation

    Answer: B. Trisodium phosphate

    Alginate gels when soluble potassium or sodium alginate reacts with calcium ions from calcium sulfate dihydrate (the reactor) to form an insoluble, cross-linked calcium alginate. If this reaction began immediately on mixing, there would be no working time. Trisodium phosphate (a retarder) is added because calcium ions react preferentially with it to form calcium phosphate. Only after the phosphate is used up do calcium ions begin cross-linking the alginate chains, so the amount of retarder determines working and setting time. Diatomaceous earth is a filler that increases strength and stiffness and gives a smooth, non-sticky mix; zinc oxide is also a filler; potassium titanium fluoride is added to counteract the inhibiting effect of alginate on the setting of gypsum, giving harder, smoother die surfaces. Clinically, warmer water shortens and colder water lengthens setting time without altering the chemistry.
    Discuss this question
  8. 68. A heat-cured denture with a very thick palatal section shows porosity confined to its centre. The most likely cause is:

    • A. Rapid heating raising the temperature above the boiling point of monomer
    • B. Insufficient packing pressure
    • C. Excessive monomer in the polymer-monomer ratio
    • D. Use of a tin-foil substitute
    Show answer & explanation

    Answer: A. Rapid heating raising the temperature above the boiling point of monomer

    Porosity in heat-processed PMMA is of two main types. Gaseous (internal) porosity occurs in thick sections when the processing temperature rises too rapidly. Polymerization of methyl methacrylate is exothermic, and in the centre of a thick mass heat cannot dissipate, so the internal temperature can exceed the boiling point of monomer (100.8 C). The monomer vaporises, forming uniform, fine spherical voids localised to the thickest areas, while thin, peripheral areas remain sound. Prevention: use a long, low-temperature curing cycle (e.g. 74 C for 8 hours or longer, then a terminal boil). Contraction porosity, by contrast, results from insufficient packing pressure or inadequate dough, and produces irregular voids distributed throughout the denture, often near the surface. Excess monomer increases shrinkage; separating medium problems cause adherence of gypsum or crazing, not central porosity.
    Discuss this question
  9. 69. Mixing zinc phosphate cement on a frozen glass slab (-6 to -10 C) is primarily done to:

    • A. Decrease the solubility of the set cement
    • B. Increase working time and allow more powder to be incorporated
    • C. Reduce the acidity of the freshly mixed cement
    • D. Increase the setting time in the mouth
    Show answer & explanation

    Answer: B. Increase working time and allow more powder to be incorporated

    The reaction between zinc oxide powder and phosphoric acid liquid is strongly exothermic, and heat accelerates the setting. Mixing on a cool or frozen slab dissipates this heat and slows the reaction, greatly increasing working time (by several minutes). Because the matrix forms more slowly, the operator can incorporate about 50-75% more powder for a given consistency, which increases strength and reduces solubility as secondary benefits. Once the cement is placed in the mouth, setting time is actually shorter than with conventional mixing, which is useful clinically, for example when cementing multiple-unit bridges. A recognised disadvantage is moisture condensation on the frozen slab, which can dilute the liquid. Powder is classically added in small increments over a large area of the slab for the same reason - to dissipate heat. The freshly mixed cement remains acidic (pH about 2 at 2 minutes) whichever technique is used.
    Discuss this question
  10. 70. Tartaric acid added to glass ionomer cement primarily:

    • A. Improves handling by increasing working time and sharpening the set
    • B. Increases fluoride release
    • C. Acts as a radiopacifier
    • D. Forms cross-links with polyacrylic acid chains
    Show answer & explanation

    Answer: A. Improves handling by increasing working time and sharpening the set

    Tartaric acid is added to the GIC liquid (or as a dried acid in the powder) to control the setting reaction. It reacts preferentially with ions released from the glass, delaying the formation of the polyacrylate matrix and so extending working time; then it promotes rapid cross-linking, giving a short, sharp setting time. The overall result is improved handling characteristics and a 'snap set'. It also improves the strength somewhat. Fluoride release comes from the fluoroaluminosilicate glass, not from tartaric acid. Radiopacity is provided by elements such as strontium, barium or lanthanum incorporated in the glass. The cross-links in the set cement are ionic salt bridges formed between carboxyl groups of the polyacid chains and calcium and aluminium cations, not by tartaric acid itself. Itaconic and maleic acids are copolymerised with acrylic acid to reduce viscosity and prevent gelation of the liquid.
    Discuss this question
  11. 71. The chemical adhesion of glass ionomer cement to tooth structure is mainly due to:

    • A. Micromechanical retention in resin tags
    • B. Covalent bonds with dentinal collagen
    • C. Formation of a hybrid layer of resin-infiltrated dentin
    • D. Chelation of calcium ions on hydroxyapatite by carboxyl groups
    Show answer & explanation

    Answer: D. Chelation of calcium ions on hydroxyapatite by carboxyl groups

    Glass ionomer (like zinc polycarboxylate) bonds chemically to enamel and dentin. The ionised carboxyl groups (COO-) of the polyacrylic acid chelate calcium ions on the surface of hydroxyapatite. During this process phosphate ions from the tooth are displaced into the cement and an intermediate ion-exchange layer forms between cement and tooth. Bond strength is therefore higher to enamel (more mineral) than to dentin. A clean surface treated with a mild polyacrylic acid conditioner (10-20%, 10-20 s) removes the smear layer without opening tubules excessively and improves bonding. Resin tags and the hybrid layer (Nakabayashi) describe micromechanical bonding of resin adhesives, not of conventional GIC. Covalent bonding with collagen has been proposed but is minor. Because of this chemical bond, fluoride release and a coefficient of thermal expansion close to tooth structure, GIC shows good marginal seal in non-retentive Class V lesions.
    Discuss this question
  12. 72. Early moisture contamination or desiccation of a conventional GIC restoration is harmful mainly because:

    • A. Fluoride release is permanently stopped
    • B. The glass particles dissolve completely in saliva
    • C. Aluminium polyacrylate matrix formation is incomplete for about 24 hours
    • D. Unreacted monomer is leached out
    Show answer & explanation

    Answer: C. Aluminium polyacrylate matrix formation is incomplete for about 24 hours

    The setting of GIC is an acid-base reaction occurring in stages. Polyacid attacks the glass, releasing Ca2+, Al3+, Na+ and F-. Calcium ions react first, forming a relatively weak calcium polyacrylate matrix within the first few minutes (initial set). Aluminium ions are released and incorporated more slowly, forming the stronger, more insoluble aluminium polyacrylate over about 24 hours, with maturation continuing for weeks. During this period the cement is vulnerable: contact with water leaches out calcium and aluminium ions and causes surface erosion and a chalky surface (water sensitivity), while drying causes loss of water needed for reaction, leading to crazing and cracking. Hence the restoration should be protected with varnish, petroleum jelly or a light-cured bonding resin immediately after setting. Fluoride release continues regardless. Conventional GIC contains no resin monomer; that concern applies to resin-modified GIC.
    Discuss this question
  13. 73. Zinc polycarboxylate cement appears very viscous yet can produce a thin film thickness because it is:

    • A. Dilatant
    • B. Newtonian
    • C. Pseudoplastic (shear-thinning)
    • D. Thixotropic only at body temperature
    Show answer & explanation

    Answer: C. Pseudoplastic (shear-thinning)

    Zinc polycarboxylate cement (zinc oxide powder with aqueous polyacrylic acid) looks thick and stiff compared with zinc phosphate at a correct mix, which often misleads clinicians into adding too much liquid. However, the mix is pseudoplastic: its viscosity decreases as shear rate increases. During mixing and particularly when a crown is seated with pressure, the high shear thins the cement so it flows readily and achieves an acceptable film thickness (about 25 micrometres). A dilatant material would become thicker with increasing shear; a Newtonian liquid has constant viscosity regardless of shear rate. Polycarboxylate was the first cement to bond chemically to tooth structure (through calcium chelation), is mild to the pulp because the large polyacrylic acid molecules penetrate dentinal tubules poorly, but has a short working time, lower compressive strength than zinc phosphate, and significant viscoelastic creep.
    Discuss this question
  14. 74. A composite restoration placed over a cavity previously temporised with a ZOE (eugenol-containing) cement shows soft, poorly cured resin. The reason is:

    • A. Eugenol increases the pH of dentin
    • B. Zinc ions react with the photoinitiator
    • C. Eugenol scavenges free radicals and inhibits polymerization
    • D. Eugenol reduces the depth of light penetration
    Show answer & explanation

    Answer: C. Eugenol scavenges free radicals and inhibits polymerization

    Eugenol is a phenolic compound. Phenolic hydroxyl groups readily donate hydrogen atoms to free radicals, forming stable radicals that do not propagate the chain. Since methacrylate-based composites, bonding agents and resin cements polymerize by free-radical addition polymerization, residual eugenol in dentin acts as an inhibitor (scavenger), producing incompletely cured, soft resin and reduced bond strength at the interface. Eugenol penetrates dentin, so even after mechanical removal of the temporary, residues can remain; thorough cleaning, acid etching and preferably non-eugenol temporary materials are recommended when a resin restoration or adhesive cementation is planned. This is also why ZOE should not be used as a base under composites. The same principle explains why hydroquinone or BHT is added to monomers as an inhibitor to prolong shelf life.
    Discuss this question
  15. 75. In a high-copper admixed amalgam, the gamma-2 phase is eliminated by its reaction with the silver-copper eutectic to form:

    • A. Cu3Sn (epsilon)
    • B. Ag2Hg3 (gamma-1)
    • C. Ag3Sn (gamma)
    • D. Cu6Sn5 (eta-prime)
    Show answer & explanation

    Answer: D. Cu6Sn5 (eta-prime)

    In conventional low-copper amalgam, Ag3Sn (gamma) reacts with mercury to form Ag2Hg3 (gamma-1) and Sn7-8Hg (gamma-2), with unreacted gamma particles remaining. Gamma-2 is the weakest, softest and most corrosion-prone phase, and its corrosion leads to marginal breakdown. In high-copper admixed alloys, silver-copper eutectic spheres are mixed with lathe-cut low-copper particles. Initially gamma-1 and gamma-2 form as usual, but gamma-2 then reacts with the copper of the Ag-Cu particles to form Cu6Sn5 (eta-prime) plus gamma-1, so little or no gamma-2 remains after about a week. In single-composition (unicompositional) high-copper alloys, Cu6Sn5 forms directly without an intermediate gamma-2 phase. Cu3Sn (epsilon) is present in some unicompositional alloy particles but is not the reaction product that consumes gamma-2. Elimination of gamma-2 improves corrosion resistance, strength, creep and marginal integrity.
    Discuss this question
  16. 76. Five days after placement of a Class II amalgam with poor isolation, the patient reports pain and the restoration is protruding. The alloy most likely:

    • A. Was a zinc-containing alloy contaminated with moisture during condensation
    • B. Was a zinc-free high-copper spherical alloy
    • C. Was over-triturated
    • D. Had excess mercury removed during condensation
    Show answer & explanation

    Answer: A. Was a zinc-containing alloy contaminated with moisture during condensation

    This is the classic picture of delayed (secondary) expansion. When a zinc-containing amalgam alloy (zinc more than 0.01%) is contaminated with moisture (saliva, blood) during trituration or condensation, zinc reacts with water to form zinc oxide and liberates hydrogen gas: Zn + H2O = ZnO + H2. The hydrogen accumulates within the restoration, building internal pressure that causes expansion beginning about 3-5 days after placement and continuing for months; expansion may exceed 4%. Clinically, this produces pressure pain, protrusion of the restoration from the cavity, marginal breakdown and increased microleakage and corrosion. Zinc-free alloys do not show this reaction, which is why they are preferred when moisture control is difficult. Over-trituration and removal of excess mercury generally reduce, not increase, dimensional change. Zinc is included in some alloys as a scavenger of oxygen during manufacture.
    Discuss this question
  17. 77. The physical property of dental amalgam that has been most closely correlated with marginal breakdown is:

    • A. Compressive strength
    • B. Dimensional change during setting
    • C. Tensile strength
    • D. Creep
    Show answer & explanation

    Answer: D. Creep

    Creep is the time-dependent plastic deformation of a material under a constant load or stress. Amalgam is used at a temperature that is a large fraction of the melting point of its phases (especially gamma-1 and gamma-2), so it creeps under masticatory stress. Classic studies (Mahler and colleagues) showed a strong correlation between static creep values and marginal breakdown ('ditching'): under repeated loading, amalgam at the margins is extruded beyond the cavity margin, the thin unsupported flash fractures and corrodes, producing a ditch. Low-copper amalgams with gamma-2 show static creep of about 0.8-8%, whereas high-copper single-composition alloys have creep values as low as about 0.05-0.1%, explaining their clinically superior marginal integrity. Compressive strength of amalgam is high and does not correlate well with marginal failure; dimensional change per ISO is small (within +/-0.15%).
    Discuss this question
  18. 78. Compared with a lathe-cut amalgam alloy, a spherical alloy:

    • A. Requires more mercury and greater condensation force
    • B. Has lower early compressive strength
    • C. Requires less mercury and less condensation force
    • D. Is unsuitable for use with a larger condenser
    Show answer & explanation

    Answer: C. Requires less mercury and less condensation force

    Spherical alloy particles have a smaller surface area per unit volume than irregular lathe-cut filings, so they are wetted by less mercury. Typical mercury content is about 40-45% for spherical alloys compared with about 48-53% for lathe-cut alloys. Spherical particles slide past one another readily during condensation, so less condensation pressure is needed; however, because the mass is less resistant to lateral displacement, larger condensers are used, and achieving tight proximal contacts in Class II cavities is more difficult (the amalgam tends to flow rather than push the matrix band). Spherical alloys also develop higher early (1-hour) compressive strength, which is an advantage for early loading. Lathe-cut and admixed alloys resist condensation more, allowing better adaptation against matrix bands and easier contact formation. These handling differences are frequently tested in clinical scenario questions.
    Discuss this question
  19. 79. Which cavity configuration has the highest C-factor and therefore the greatest polymerization shrinkage stress in a composite restoration?

    • A. Class I occlusal
    • B. Class IV incisal angle
    • C. Class II MO
    • D. Labial veneer on a flat surface
    Show answer & explanation

    Answer: A. Class I occlusal

    The configuration factor (C-factor), described by Feilzer and Davidson, is the ratio of bonded to unbonded (free) surfaces of a restoration. Unbonded surfaces allow the composite to flow during the pre-gel phase and relieve shrinkage stress, whereas bonded surfaces restrain it. A Class I occlusal box has five bonded walls (mesial, distal, buccal, lingual and pulpal floor) and only one free surface, giving a C-factor of 5, the highest among common cavities, so it develops the greatest shrinkage stress, risk of debonding, cuspal flexure and postoperative sensitivity. A Class II MO has about 4 bonded to 2 free surfaces (C about 2), a Class IV has a very low value (about 0.5), and a flat veneer surface is about 0.2. Clinical strategies to reduce stress in high C-factor cavities include incremental layering (oblique increments of 2 mm), use of flowable or GIC liners, soft-start curing and bulk-fill low-stress composites.
    Discuss this question
  20. 80. Microfilled composites cannot achieve high inorganic filler loading mainly because:

    • A. The particles are too large to be silanated
    • B. Colloidal silica has a very high surface area that greatly increases viscosity
    • C. Colloidal silica is radiolucent
    • D. Microfillers inhibit free-radical polymerization
    Show answer & explanation

    Answer: B. Colloidal silica has a very high surface area that greatly increases viscosity

    Microfilled composites use pyrogenic (colloidal) silica of about 0.04 micrometre particle size. Such tiny particles have an enormous surface area per unit weight (about 50-400 square metres per gram). Each particle surface must be wetted by resin, so even a modest amount of filler drastically increases viscosity, making it impossible to load directly beyond about 25% by weight. Manufacturers overcome this with prepolymerized (organic) fillers: highly filled resin is polymerized, ground into particles and added to more resin, raising overall inorganic content to about 35-60% by weight. Consequently, microfills have higher polymerization shrinkage, higher coefficient of thermal expansion, higher water sorption and lower modulus and strength than hybrids, but they give the best polish and surface lustre retention. They are suitable for Class V and anterior aesthetic areas, but not for stress-bearing Class IV or posterior restorations. Silanation and radiopacity are not the limiting factors.
    Discuss this question