Five days after placement of a Class II amalgam with poor isolation, the patient reports pain and the restoration is protruding. The alloy most likely:

21 views
  • Was a zinc-containing alloy contaminated with moisture during condensation (Correct Answer)
  • Was a zinc-free high-copper spherical alloy
  • Was over-triturated
  • Had excess mercury removed during condensation

Explanation

This is the classic picture of delayed (secondary) expansion. When a zinc-containing amalgam alloy (zinc more than 0.01%) is contaminated with moisture (saliva, blood) during trituration or condensation, zinc reacts with water to form zinc oxide and liberates hydrogen gas: Zn + H2O = ZnO + H2. The hydrogen accumulates within the restoration, building internal pressure that causes expansion beginning about 3-5 days after placement and continuing for months; expansion may exceed 4%. Clinically, this produces pressure pain, protrusion of the restoration from the cavity, marginal breakdown and increased microleakage and corrosion. Zinc-free alloys do not show this reaction, which is why they are preferred when moisture control is difficult. Over-trituration and removal of excess mercury generally reduce, not increase, dimensional change. Zinc is included in some alloys as a scavenger of oxygen during manufacture.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs