Microfilled composites cannot achieve high inorganic filler loading mainly because:

21 views
  • The particles are too large to be silanated
  • Colloidal silica has a very high surface area that greatly increases viscosity (Correct Answer)
  • Colloidal silica is radiolucent
  • Microfillers inhibit free-radical polymerization

Explanation

Microfilled composites use pyrogenic (colloidal) silica of about 0.04 micrometre particle size. Such tiny particles have an enormous surface area per unit weight (about 50-400 square metres per gram). Each particle surface must be wetted by resin, so even a modest amount of filler drastically increases viscosity, making it impossible to load directly beyond about 25% by weight. Manufacturers overcome this with prepolymerized (organic) fillers: highly filled resin is polymerized, ground into particles and added to more resin, raising overall inorganic content to about 35-60% by weight. Consequently, microfills have higher polymerization shrinkage, higher coefficient of thermal expansion, higher water sorption and lower modulus and strength than hybrids, but they give the best polish and surface lustre retention. They are suitable for Class V and anterior aesthetic areas, but not for stress-bearing Class IV or posterior restorations. Silanation and radiopacity are not the limiting factors.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs