The physical property of dental amalgam that has been most closely correlated with marginal breakdown is:
- Compressive strength
- Dimensional change during setting
- Tensile strength
- Creep (Correct Answer)
Explanation
Creep is the time-dependent plastic deformation of a material under a constant load or stress. Amalgam is used at a temperature that is a large fraction of the melting point of its phases (especially gamma-1 and gamma-2), so it creeps under masticatory stress. Classic studies (Mahler and colleagues) showed a strong correlation between static creep values and marginal breakdown ('ditching'): under repeated loading, amalgam at the margins is extruded beyond the cavity margin, the thin unsupported flash fractures and corrodes, producing a ditch. Low-copper amalgams with gamma-2 show static creep of about 0.8-8%, whereas high-copper single-composition alloys have creep values as low as about 0.05-0.1%, explaining their clinically superior marginal integrity. Compressive strength of amalgam is high and does not correlate well with marginal failure; dimensional change per ISO is small (within +/-0.15%).