Dental Materials MCQs for Dental NMCLE / Loksewa / MDS Exams – Page 5
90 Dental Materials multiple-choice questions with answers and explanations, from the ExamsNepal question bank for Dental NMCLE / Loksewa / MDS Exams. Try each question first, then open the answer to check your reasoning.
Preparing for MDS Entrance Exam (Master of Dental Surgery)? See the exam pattern, syllabus and free mock tests.
81. A composite containing TPO (Lucirin) as photoinitiator cures poorly with a single-peak blue LED (450-470 nm). The reason is:
- A. TPO requires a tertiary amine that blue light destroys
- B. TPO absorbs maximally at 468 nm
- C. TPO absorbs maximally in the violet range (about 380-410 nm)
- D. LED light generates too little heat
Discuss this questionShow answer & explanation
Answer: C. TPO absorbs maximally in the violet range (about 380-410 nm)
Camphorquinone (CQ), the most common photoinitiator, absorbs blue light between about 400 and 500 nm with a peak around 468 nm and requires a tertiary amine co-initiator to generate free radicals. Because CQ is yellow, it can affect the colour of very light (bleach) shades, so manufacturers add or substitute alternative initiators such as TPO (Lucirin TPO, a monoacylphosphine oxide), PPD (phenylpropanedione) or Ivocerin. These absorb mainly in the violet or near-UV region: TPO peaks at about 380-410 nm. First- and second-generation LED units emit a narrow band centred around 450-470 nm, which matches CQ well but poorly overlaps TPO absorption, leading to inadequate curing. Polywave (multi-peak) LEDs with an additional violet emission, or QTH units with a broad spectrum, are required. TPO does not need an amine co-initiator. Heat output is not the limiting factor in photoinitiation.82. Over-drying acid-etched dentin before applying an acetone-based primer mainly reduces bond strength because:
- A. The smear plugs reform and occlude the tubules
- B. Acetone evaporates before reaching the dentin
- C. Calcium phosphate precipitates on the surface
- D. The demineralized collagen network collapses, preventing resin infiltration
Discuss this questionShow answer & explanation
Answer: D. The demineralized collagen network collapses, preventing resin infiltration
Phosphoric acid etching removes the smear layer and demineralizes the superficial 3-7 micrometres of intertubular and peritubular dentin, leaving a network of exposed collagen fibrils supported by water. If the dentin is air-dried excessively, the water evaporates and the collagen fibres collapse into a dense, compact layer, closing the interfibrillar spaces through which the primer and adhesive monomers must diffuse. Resin then fails to infiltrate fully, forming a poor hybrid layer with reduced bond strength, nanoleakage and postoperative sensitivity. This is the basis of the 'wet bonding' technique (Kanca), in which etched dentin is kept visibly moist. Acetone-based systems are most sensitive because acetone has strong water-chasing ability but cannot re-expand a collapsed network, whereas water-based primers can partly re-expand collagen. Excessive wetness ('over-wet') causes phase separation of monomers, so a glistening, moist surface is ideal.83. Superelasticity of nickel-titanium archwires is a result of:
- A. Work hardening during cold drawing
- B. Precipitation hardening by titanium carbides
- C. Ordering of the beta-titanium lattice
- D. Stress-induced transformation from austenite to martensite
Discuss this questionShow answer & explanation
Answer: D. Stress-induced transformation from austenite to martensite
NiTi (nitinol) alloys exist in two main crystalline phases: austenite (body-centred cubic, stable at higher temperature and lower stress) and martensite (monoclinic, stable at lower temperature or higher stress). In austenitic 'superelastic' wires, when the wire is activated (deflected) in the mouth the applied stress induces a transformation from austenite to martensite. This transformation accommodates large strains (up to about 8-10%) with very little increase in stress, producing the flat 'plateau' region of the load-deflection curve. On unloading, martensite reverts to austenite and the wire returns to its original shape while delivering a nearly constant, light force over a wide range of tooth movement. Shape memory, in contrast, involves thermally induced transformation (martensite to austenite on heating above the transition temperature). Beta-titanium (TMA) gets its properties from a different alloy system; work hardening is the strengthening mechanism of stainless steel.84. Soldering an 18-8 stainless steel appliance for a prolonged time at about 650 C makes it prone to intergranular corrosion due to:
- A. Loss of nickel by oxidation
- B. Chromium carbide precipitation at grain boundaries
- C. Transformation of austenite to martensite
- D. Formation of a thick passivating oxide film
Discuss this questionShow answer & explanation
Answer: B. Chromium carbide precipitation at grain boundaries
18-8 austenitic stainless steel contains about 18% chromium and 8% nickel with a small amount of carbon. Its corrosion resistance depends on a thin, passive chromium oxide film, which requires at least about 12-13% chromium in solid solution. When the steel is heated in the range of roughly 400-900 C (the sensitization range) for a sufficient time, as during prolonged soldering or welding, carbon diffuses to grain boundaries and combines with chromium to form chromium carbide (Cr23C6). The zones adjacent to grain boundaries become depleted of chromium, lose passivity and corrode preferentially (intergranular corrosion, 'weld decay'). The steel is said to be sensitized. Prevention: keep soldering time short with low-fusing silver solders and a fluoride-containing flux, reduce carbon content, or use stabilized steel containing titanium (or niobium), which forms titanium carbide preferentially and keeps chromium in solution.85. Gypsum-bonded investments should not be heated above about 700 C because:
- A. Silica undergoes inversion and contracts
- B. The investment loses all its hygroscopic expansion
- C. Calcium sulfate decomposes, releasing sulfur gases that contaminate the casting
- D. Cristobalite converts to quartz
Discuss this questionShow answer & explanation
Answer: C. Calcium sulfate decomposes, releasing sulfur gases that contaminate the casting
Gypsum-bonded investments consist of calcium sulfate hemihydrate as binder and silica (quartz and/or cristobalite) as refractory, along with chemical modifiers such as carbon or reducing agents. Calcium sulfate is thermally unstable at high temperatures. Above about 700 C, particularly in the presence of carbon, it reacts and decomposes, liberating sulfur dioxide and sulfur trioxide gases. These gases contaminate and embrittle gold castings (sulfide contamination) and produce rough surfaces. Hence these investments are limited to burnout at about 650-700 C and are suitable mainly for conventional gold alloys with low melting ranges. High-fusing alloys such as metal-ceramic and base metal alloys need phosphate-bonded or silica-bonded investments that tolerate higher temperatures. Silica polymorphs (quartz, cristobalite) undergo inversion with expansion on heating, which is beneficial for compensating shrinkage; this is not the limiting factor.86. Base metal crowns cast in a phosphate-bonded investment are consistently too tight on the dies. The most appropriate correction is to:
- A. Dilute the special liquid with water
- B. Increase the concentration of the colloidal silica special liquid
- C. Decrease the burnout temperature
- D. Use a thinner ring liner
Discuss this questionShow answer & explanation
Answer: B. Increase the concentration of the colloidal silica special liquid
Phosphate-bonded investments set by an acid-base reaction between monoammonium phosphate (NH4H2PO4) and magnesium oxide, forming a hydrated magnesium ammonium phosphate binder, with silica as refractory. On heating, further reactions and silica inversion contribute to thermal expansion. These investments are mixed with a special liquid that is an aqueous suspension of colloidal silica. Colloidal silica increases both setting and thermal expansion, so the total expansion can be adjusted by changing its concentration: using undiluted special liquid gives maximum expansion, while diluting it with water reduces expansion. A casting that is too tight indicates insufficient mold expansion to compensate for alloy solidification shrinkage, so the concentration of special liquid should be increased (less dilution). Reducing burnout temperature would lower thermal expansion and worsen fit; a thinner liner restricts setting expansion. These investments tolerate high burnout temperatures needed for base metal and metal-ceramic alloys.87. In high-noble metal-ceramic alloys, a chemical bond with porcelain is provided by oxides of trace elements such as:
- A. Tin, indium and iron
- B. Gold and platinum
- C. Palladium and silver
- D. Copper and zinc
Discuss this questionShow answer & explanation
Answer: A. Tin, indium and iron
The metal-ceramic bond has several components: mechanical interlocking, compressive forces from thermal expansion mismatch, van der Waals forces and, most importantly, chemical bonding through a metal oxide layer. Noble metals such as gold, platinum and palladium do not readily form oxides. Therefore small amounts (often less than 1%) of oxidizable base metals such as tin, indium and iron (and gallium in palladium-based alloys) are added. During the degassing (oxidation) heat treatment, these elements diffuse to the surface and form a thin, adherent oxide layer. When opaque porcelain is fused, the oxides partially dissolve into the glass, establishing a chemical bond across the interface. An overly thick oxide layer weakens the bond, as cohesive failure then occurs within the oxide. Silver is undesirable in such alloys because it causes 'greening' (discolouration) of porcelain. Copper is avoided because its oxides discolour porcelain.88. For a sound metal-ceramic restoration, the coefficient of thermal expansion of the alloy should be:
- A. Slightly higher than that of porcelain
- B. Considerably lower than that of porcelain
- C. Slightly lower than that of porcelain
- D. Several times higher than that of porcelain
Discuss this questionShow answer & explanation
Answer: A. Slightly higher than that of porcelain
Porcelain is strong in compression but weak in tension. When a metal-ceramic restoration cools from the firing temperature, both components contract. If the alloy has a slightly higher coefficient of thermal expansion (CTE), typically by about 0.5-1.0 x 10^-6 per degree C, it contracts slightly more than the porcelain, placing the porcelain under mild residual compressive stress and the metal under tension. This compressive stress helps resist crack propagation and improves the strength of the veneer. If the alloy CTE were lower than porcelain, the porcelain would be left in tension, causing immediate or delayed cracking (crazing). If the mismatch were too large in either direction, stresses would exceed the strength of the porcelain or the bond, leading to cracking or delamination. Hence alloy and porcelain systems must be carefully matched, and additional firings that alter porcelain CTE (leucite content) should be minimized.89. Transformation toughening in yttria-stabilized tetragonal zirconia (Y-TZP) involves:
- A. Tetragonal to monoclinic transformation with about 3-5% volume expansion
- B. Monoclinic to tetragonal transformation with volume contraction
- C. Cubic to tetragonal transformation with crack branching
- D. Leucite crystallization at the crack tip
Discuss this questionShow answer & explanation
Answer: A. Tetragonal to monoclinic transformation with about 3-5% volume expansion
Pure zirconia exists as monoclinic at room temperature, tetragonal above about 1170 C and cubic above about 2370 C. Addition of about 3 mol% yttria allows the metastable tetragonal phase to be retained at room temperature (Y-TZP). When a crack propagates, the high tensile stress field at the crack tip triggers transformation of tetragonal grains to the monoclinic phase, accompanied by a volume expansion of about 3-5%. This expansion generates compressive stresses around the crack tip that oppose its opening and slow propagation, greatly increasing fracture toughness (about 5-10 MPa m^0.5). The same transformation can occur slowly at the surface in the presence of water at low temperature (low-temperature degradation or ageing), causing roughening and microcracking; grinding and sandblasting can also trigger it. Leucite reinforcement is a mechanism of glass ceramics, and cubic zirconia (in high-translucency 5Y-PSZ) shows less transformation toughening.90. For adhesive cementation of a monolithic zirconia crown, the most reliable surface treatment is:
- A. 5% hydrofluoric acid etching followed by silane
- B. 37% phosphoric acid etching followed by silane
- C. Airborne-particle abrasion with alumina followed by an MDP-containing primer or cement
- D. Silane application alone without abrasion
Discuss this questionShow answer & explanation
Answer: C. Airborne-particle abrasion with alumina followed by an MDP-containing primer or cement
Zirconia is a polycrystalline ceramic with no glassy phase, so it cannot be etched by hydrofluoric acid; HF etching followed by silane is the protocol for glass-matrix ceramics such as feldspathic porcelain and lithium disilicate (5% HF for about 20 s). Silane couples to silica-based surfaces and is ineffective on pure zirconia. The most reliable, evidence-based protocol (e.g. the 'APC concept') is airborne-particle abrasion with fine alumina (about 50 micrometres) at low pressure (about 1-2 bar) to clean and roughen the surface, followed by a primer or resin cement containing the phosphate monomer 10-MDP, which forms chemical bonds with zirconium oxide. Tribochemical silica coating followed by silane is an alternative. Phosphoric acid does not etch zirconia and saliva contamination is best removed with dedicated cleaning pastes, since phosphate contamination occupies the bonding sites. Excessive abrasion pressure may induce phase transformation and microcracks.