A heat-cured denture with a very thick palatal section shows porosity confined to its centre. The most likely cause is:
- Rapid heating raising the temperature above the boiling point of monomer (Correct Answer)
- Insufficient packing pressure
- Excessive monomer in the polymer-monomer ratio
- Use of a tin-foil substitute
Explanation
Porosity in heat-processed PMMA is of two main types. Gaseous (internal) porosity occurs in thick sections when the processing temperature rises too rapidly. Polymerization of methyl methacrylate is exothermic, and in the centre of a thick mass heat cannot dissipate, so the internal temperature can exceed the boiling point of monomer (100.8 C). The monomer vaporises, forming uniform, fine spherical voids localised to the thickest areas, while thin, peripheral areas remain sound. Prevention: use a long, low-temperature curing cycle (e.g. 74 C for 8 hours or longer, then a terminal boil). Contraction porosity, by contrast, results from insufficient packing pressure or inadequate dough, and produces irregular voids distributed throughout the denture, often near the surface. Excess monomer increases shrinkage; separating medium problems cause adherence of gypsum or crazing, not central porosity.