Which elastomeric impression material shows the highest elastic recovery (least permanent deformation) after removal from undercuts?
- Addition silicone (Correct Answer)
- Polysulfide
- Condensation silicone
- Polyether
Explanation
Elastic recovery is tested by compressing the set material (e.g. 12% strain for 30 s) and measuring residual deformation. Addition silicone (PVS) shows the best recovery, about 99.5-99.9% (permanent deformation roughly 0.05-0.4%), because its highly cross-linked network formed by addition polymerization is very elastic. Polyether follows closely (about 98.5-99%), condensation silicone around 98.5-99.5%, while polysulfide is the poorest (about 96-97%) owing to its more viscoelastic, less cross-linked structure, which is why polysulfide impressions should be removed with a quick snap and poured within an hour. Clinically, a material with high elastic recovery tolerates deeper undercuts and delayed or multiple pours. Addition silicone also has the best dimensional stability because no by-product is lost, making it the material of choice when pouring may be delayed.