In a high-copper admixed amalgam, the gamma-2 phase is eliminated by its reaction with the silver-copper eutectic to form:
- Cu3Sn (epsilon)
- Ag2Hg3 (gamma-1)
- Ag3Sn (gamma)
- Cu6Sn5 (eta-prime) (Correct Answer)
Explanation
In conventional low-copper amalgam, Ag3Sn (gamma) reacts with mercury to form Ag2Hg3 (gamma-1) and Sn7-8Hg (gamma-2), with unreacted gamma particles remaining. Gamma-2 is the weakest, softest and most corrosion-prone phase, and its corrosion leads to marginal breakdown. In high-copper admixed alloys, silver-copper eutectic spheres are mixed with lathe-cut low-copper particles. Initially gamma-1 and gamma-2 form as usual, but gamma-2 then reacts with the copper of the Ag-Cu particles to form Cu6Sn5 (eta-prime) plus gamma-1, so little or no gamma-2 remains after about a week. In single-composition (unicompositional) high-copper alloys, Cu6Sn5 forms directly without an intermediate gamma-2 phase. Cu3Sn (epsilon) is present in some unicompositional alloy particles but is not the reaction product that consumes gamma-2. Elimination of gamma-2 improves corrosion resistance, strength, creep and marginal integrity.