A stone die poured 5 minutes after taking an addition silicone impression shows multiple small surface voids. The most likely cause is:

27 views
  • Sulfur contamination from latex gloves
  • Release of hydrogen gas from the impression (Correct Answer)
  • Release of ethanol by-product
  • Imbibition of water by the impression

Explanation

Addition silicone (polyvinyl siloxane) sets by a platinum-catalysed hydrosilation reaction between vinyl-terminated siloxane and silane (Si-H) groups. There is no reaction by-product, which is why the material has excellent dimensional stability. However, if residual Si-H groups or moisture are present, a secondary reaction can release hydrogen gas from the set impression for some time after setting. If gypsum is poured too early, the evolved hydrogen produces pinpoint voids on the die surface. Remedies are to delay pouring (classically 1-2 hours) or to use products containing hydrogen scavengers such as finely divided palladium, which can be poured immediately. Ethanol release and shrinkage are features of condensation silicone; water as by-product is from polysulfide; imbibition is a problem of polyether and hydrocolloids. Latex sulfur contamination causes inhibition of setting (tacky surface), not voids in the die.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs