For adhesive cementation of a monolithic zirconia crown, the most reliable surface treatment is:
- 5% hydrofluoric acid etching followed by silane
- 37% phosphoric acid etching followed by silane
- Airborne-particle abrasion with alumina followed by an MDP-containing primer or cement (Correct Answer)
- Silane application alone without abrasion
Explanation
Zirconia is a polycrystalline ceramic with no glassy phase, so it cannot be etched by hydrofluoric acid; HF etching followed by silane is the protocol for glass-matrix ceramics such as feldspathic porcelain and lithium disilicate (5% HF for about 20 s). Silane couples to silica-based surfaces and is ineffective on pure zirconia. The most reliable, evidence-based protocol (e.g. the 'APC concept') is airborne-particle abrasion with fine alumina (about 50 micrometres) at low pressure (about 1-2 bar) to clean and roughen the surface, followed by a primer or resin cement containing the phosphate monomer 10-MDP, which forms chemical bonds with zirconium oxide. Tribochemical silica coating followed by silane is an alternative. Phosphoric acid does not etch zirconia and saliva contamination is best removed with dedicated cleaning pastes, since phosphate contamination occupies the bonding sites. Excessive abrasion pressure may induce phase transformation and microcracks.