Over-drying acid-etched dentin before applying an acetone-based primer mainly reduces bond strength because:

20 views
  • The smear plugs reform and occlude the tubules
  • Acetone evaporates before reaching the dentin
  • Calcium phosphate precipitates on the surface
  • The demineralized collagen network collapses, preventing resin infiltration (Correct Answer)

Explanation

Phosphoric acid etching removes the smear layer and demineralizes the superficial 3-7 micrometres of intertubular and peritubular dentin, leaving a network of exposed collagen fibrils supported by water. If the dentin is air-dried excessively, the water evaporates and the collagen fibres collapse into a dense, compact layer, closing the interfibrillar spaces through which the primer and adhesive monomers must diffuse. Resin then fails to infiltrate fully, forming a poor hybrid layer with reduced bond strength, nanoleakage and postoperative sensitivity. This is the basis of the 'wet bonding' technique (Kanca), in which etched dentin is kept visibly moist. Acetone-based systems are most sensitive because acetone has strong water-chasing ability but cannot re-expand a collapsed network, whereas water-based primers can partly re-expand collagen. Excessive wetness ('over-wet') causes phase separation of monomers, so a glistening, moist surface is ideal.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs