Soldering an 18-8 stainless steel appliance for a prolonged time at about 650 C makes it prone to intergranular corrosion due to:

24 views
  • Loss of nickel by oxidation
  • Chromium carbide precipitation at grain boundaries (Correct Answer)
  • Transformation of austenite to martensite
  • Formation of a thick passivating oxide film

Explanation

18-8 austenitic stainless steel contains about 18% chromium and 8% nickel with a small amount of carbon. Its corrosion resistance depends on a thin, passive chromium oxide film, which requires at least about 12-13% chromium in solid solution. When the steel is heated in the range of roughly 400-900 C (the sensitization range) for a sufficient time, as during prolonged soldering or welding, carbon diffuses to grain boundaries and combines with chromium to form chromium carbide (Cr23C6). The zones adjacent to grain boundaries become depleted of chromium, lose passivity and corrode preferentially (intergranular corrosion, 'weld decay'). The steel is said to be sensitized. Prevention: keep soldering time short with low-fusing silver solders and a fluoride-containing flux, reduce carbon content, or use stabilized steel containing titanium (or niobium), which forms titanium carbide preferentially and keeps chromium in solution.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs