For a sound metal-ceramic restoration, the coefficient of thermal expansion of the alloy should be:
- Slightly higher than that of porcelain (Correct Answer)
- Considerably lower than that of porcelain
- Slightly lower than that of porcelain
- Several times higher than that of porcelain
Explanation
Porcelain is strong in compression but weak in tension. When a metal-ceramic restoration cools from the firing temperature, both components contract. If the alloy has a slightly higher coefficient of thermal expansion (CTE), typically by about 0.5-1.0 x 10^-6 per degree C, it contracts slightly more than the porcelain, placing the porcelain under mild residual compressive stress and the metal under tension. This compressive stress helps resist crack propagation and improves the strength of the veneer. If the alloy CTE were lower than porcelain, the porcelain would be left in tension, causing immediate or delayed cracking (crazing). If the mismatch were too large in either direction, stresses would exceed the strength of the porcelain or the bond, leading to cracking or delamination. Hence alloy and porcelain systems must be carefully matched, and additional firings that alter porcelain CTE (leucite content) should be minimized.