Transformation toughening in yttria-stabilized tetragonal zirconia (Y-TZP) involves:

19 views
  • Tetragonal to monoclinic transformation with about 3-5% volume expansion (Correct Answer)
  • Monoclinic to tetragonal transformation with volume contraction
  • Cubic to tetragonal transformation with crack branching
  • Leucite crystallization at the crack tip

Explanation

Pure zirconia exists as monoclinic at room temperature, tetragonal above about 1170 C and cubic above about 2370 C. Addition of about 3 mol% yttria allows the metastable tetragonal phase to be retained at room temperature (Y-TZP). When a crack propagates, the high tensile stress field at the crack tip triggers transformation of tetragonal grains to the monoclinic phase, accompanied by a volume expansion of about 3-5%. This expansion generates compressive stresses around the crack tip that oppose its opening and slow propagation, greatly increasing fracture toughness (about 5-10 MPa m^0.5). The same transformation can occur slowly at the surface in the presence of water at low temperature (low-temperature degradation or ageing), causing roughening and microcracking; grinding and sandblasting can also trigger it. Leucite reinforcement is a mechanism of glass ceramics, and cubic zirconia (in high-translucency 5Y-PSZ) shows less transformation toughening.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs