Base metal crowns cast in a phosphate-bonded investment are consistently too tight on the dies. The most appropriate correction is to:

24 views
  • Dilute the special liquid with water
  • Increase the concentration of the colloidal silica special liquid (Correct Answer)
  • Decrease the burnout temperature
  • Use a thinner ring liner

Explanation

Phosphate-bonded investments set by an acid-base reaction between monoammonium phosphate (NH4H2PO4) and magnesium oxide, forming a hydrated magnesium ammonium phosphate binder, with silica as refractory. On heating, further reactions and silica inversion contribute to thermal expansion. These investments are mixed with a special liquid that is an aqueous suspension of colloidal silica. Colloidal silica increases both setting and thermal expansion, so the total expansion can be adjusted by changing its concentration: using undiluted special liquid gives maximum expansion, while diluting it with water reduces expansion. A casting that is too tight indicates insufficient mold expansion to compensate for alloy solidification shrinkage, so the concentration of special liquid should be increased (less dilution). Reducing burnout temperature would lower thermal expansion and worsen fit; a thinner liner restricts setting expansion. These investments tolerate high burnout temperatures needed for base metal and metal-ceramic alloys.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs