Why should the cavosurface margin of an amalgam preparation be finished as a butt joint of about 90 degrees rather than bevelled?

30 views
  • Amalgam has low edge strength, so thin edges at a bevelled margin fracture and cause ditching (Correct Answer)
  • Bevelled margins remove too little enamel to support the restoration
  • A bevel increases the surface area available for chemical bonding of amalgam
  • A 90-degree margin causes the amalgam to expand and seal the margin better

Explanation

Amalgam is brittle. It has high compressive strength (over 350 MPa for high-copper alloys) but low tensile strength (about 50-60 MPa) and poor edge strength. If the cavosurface margin is bevelled, the amalgam at the margin is thin (an acute amalgam margin angle). This thin edge fractures under occlusal load, leaving a gap along the margin ("ditching") that promotes plaque, leakage and secondary caries. To avoid this, amalgam preparations should have a cavosurface angle that gives an amalgam margin angle of 80-90 degrees or more, a butt-joint relationship, and at least 1.5-2 mm of bulk in areas under occlusal stress. Occlusal walls slightly converge towards the occlusal surface (for retention), and the enamel walls must still be supported by dentin. The gingival margin of a Class II box is lightly planed to remove unsupported enamel rods, without a true bevel. In contrast, cast gold restorations are bevelled because gold alloy is ductile and its thin margins can be burnished to adapt to the tooth. Composite restorations can use enamel bevels to increase the surface area for etching and improve aesthetic blending, except on occlusal surfaces.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs