Which of following process removes the excess water & reduce firing shrinkage during manipulation of dental ceramic?

31 views
  • Condensation (Correct Answer)
  • Preheating
  • Firing
  • Glazing

Explanation

Manipulation of dental ceramic:
i.Condensation; process of packing the powder together. Permits to minimize porosity, improve strength, reduce
firing shrinkage & removal of excess water.
3 methods of condensation:
Vibration method
Spatulation method
Brush method
ii.Preheating procedure: for 5mins at 650°C before placing into furnace for firing procedure
Also permit remaining water vapour to dissipate
Placed directly into hot furnace for firing, result in rapid production of steam thereby voids or fracturing large section of veneer.
iii.Sintering/firing procedure: to fuse powder particle together to form a continuous mass
In metal-ceramic restoration minimum of three firing procedure are required.
iv.Glazing procedure: to provide glossy surface to ceramics 2 types:
Over glaze: separate glaze layer is applied. Chemical durability of over glaze is lower as it contain high flux content
Self or auto glaze: restoration is subject to a controlled heating at is fusion temperature
Objective of glazing:
Enhance esthetics & hygiene
Improves strength & fracture resistance
v.Cooling of porcelain: critical stage of fabrication of surface ceramic metal restoration
Rapid or very slow cooling: causes crazing on surface due to uneven thermal expansion.
@Coefficient of thermal expansion of metal ceramic on surface alloy is more than or equal to porcelain but not less.