Which alloy phase is associated with the highest strength in a type III gold alloy used for crowns?

13 views
  • Eutectic phase
  • Alpha (solid solution) phase
  • Beta (intermetallic) phase (Correct Answer)
  • Gamma-2 phase

Explanation

In dental alloys, intermetallic phases (beta, gamma', etc.) often provide increased strength and hardness compared to the softer alpha solid solution. Gamma-2 is a tin–silver phase associated with corrosion in some amalgams; eutectic refers to a low-melting mixture. The presence and nature of intermetallic phases (e.g., Au–Cu) influence mechanical properties.