Type IV die stone (improved stone) is stronger and harder than Type II model plaster mainly because:

21 views
  • Its dense, regular alpha-hemihydrate particles need less mixing water, giving less porosity in the set gypsum (Correct Answer)
  • It contains a different chemical compound that sets by polymerisation
  • It is fired at a high temperature after setting to increase strength
  • It uses a higher water/powder ratio, which dissolves more calcium sulphate

Explanation

All dental gypsum products are calcium sulphate hemihydrate (CaSO4.1/2H2O), which reacts with water to form calcium sulphate dihydrate (gypsum): the dihydrate crystals grow as interlocking needles. Differences in strength come from how the hemihydrate is made and the amount of water needed to mix it. Model plaster (Type II) is beta-hemihydrate, made by heating gypsum in an open kettle (calcination). Its particles are irregular, spongy and porous, so it needs a lot of water (water/powder ratio of about 0.45-0.50) to make a workable mix. Dental stone (Type III) and die stone (Type IV, and high-expansion Type V) are alpha-hemihydrate, made by heating gypsum under steam pressure in an autoclave, or by boiling in a calcium chloride solution for the densite form. Their particles are dense, regular and prism-shaped, so they need less water (about 0.28-0.30 for Type III and 0.22-0.24 for Type IV). Only about 0.186 g of water per gram of hemihydrate is needed for the chemical reaction. Excess water evaporates, leaving voids that weaken the set material. With less excess water, die stone has lower porosity and higher compressive strength and surface hardness. Wet strength is lower than dry strength. Accelerators (potassium sulphate, slurry of gypsum) and retarders (borax, citrates) control setting.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs