The gamma-2 phase in low-copper dental amalgam is undesirable because it is the weakest and most corrosion-prone phase. Its composition, and the phase formed instead in high-copper amalgams, are:
- Ag3Sn; replaced by the gamma-1 phase Ag2Hg3
- Ag2Hg3; replaced by the epsilon phase Cu3Sn
- Cu6Sn5; replaced by the gamma-2 phase Sn7-8Hg
- Sn7-8Hg; replaced by the eta phase Cu6Sn5 (Correct Answer)
Explanation
In conventional low-copper amalgam, the alloy particles are mainly the gamma phase (Ag3Sn). When they react with mercury, they form the gamma-1 matrix (Ag2Hg3) and the gamma-2 phase (Sn7-8Hg), with unreacted gamma particles still embedded: gamma + Hg gives gamma-1 + gamma-2 + unreacted gamma. The gamma-2 phase is the weakest and softest phase and the most prone to corrosion. Its corrosion releases mercury and leaves porosity. This causes marginal breakdown ("ditching") and a lower strength of the restoration, and tin oxides and chlorides form. High-copper amalgams (over 6% copper), either admixed (with silver-copper eutectic particles) or single-composition (spherical ternary Ag-Sn-Cu), prevent this. In admixed alloys, gamma-2 forms first and then reacts with the Ag-Cu particles to produce the eta phase (Cu6Sn5) and more gamma-1. In single-composition alloys eta forms directly, and gamma-2 is essentially absent. As a result, high-copper amalgams have better corrosion resistance, higher early compressive strength, lower creep (under 1%) and better marginal integrity. Epsilon (Cu3Sn) is found in the alloy particles.