The factor contributing for contraction of dental amalgam except?
- Low mercury alloy ratio
- Higher condensation process
- Larger alloy particle size (Correct Answer)
- More trituration
Explanation
Smaller particle consumes more mercury because of
increased surface area faster growth of gamma 1
phase favours contraction . :
Since final volume of gamma 1 is less than initial volume of
silver & mercury that go into making gamma 1. Longer
Trituration time accelerate setting which favours
contraction
Higher mercury to alloy ratio provide plastic matrix, where
expansion will occurs when gamma 1 crystal impinge on each
other producing outward pressure. After rigid gamma 1
matrix has formed, growth of gamma 1 crystal cannot force
matrix to expand, instead gamma 1 crystal will grow into
intensities containing mercury & producing continued
reaction. So, reducing mercury in mix will favour
contraction.
Note: ADA specification No.1 amalgam should neither be
contract nor expand more than 20pm/jcm after beginning
of trituration @(0.1-0.15%) between 5 minutes to 24 hrs
at 37°C.