The burn out time during casting of gold alloy is?
27 views
- 1 1/2hrs (Correct Answer)
- 1 hrs
- 30min
- 20min
Explanation
For noble metal alloys it is about 30-40mins.
In case of gypsum bonded investment for casting gold
alloys, , mould are placed in furnace & heated slowly ¢o
650-700°C for 1hr & maintained for further 30mins. This is
called low heat hygroscopic technique or two stage
burnout and expansion technique.
In case of casting noble metal alloys, mould are placed into
preheated oven at 700-850°C & hold for 30 mins. This is
called high-heat thermal expansion technique or
single stage burnout & expansion technique.