In the fabrication of CAD/CAM ceramic restorations, which sintering parameter for zirconia blocks MOST significantly affects the final restoration's fit and marginal accuracy?

32 views
  • Heating rate during sintering
  • Maximum sintering temperature
  • Cooling rate after sintering
  • Sintering shrinkage compensation during CAD design (Correct Answer)

Explanation

Pre-sintered zirconia blocks are machined in an enlarged "green" or "white" state, then sintered at 1400-1500°C, causing approximately 20-25% linear shrinkage as the porous structure densifies. If CAD software doesn't accurately compensate for this sintering shrinkage during design phase (by enlarging the milling dimensions proportionally), the final restoration will be undersized with open margins. Modern CAD systems use manufacturer-specific shrinkage factors (typically 1.20-1.25×) to ensure proper fit after sintering.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs