In metal-ceramic restorations using high-noble gold alloys, the chemical bond between porcelain and metal depends on:

18 views
  • Oxides of trace elements such as tin, indium and iron formed during the degassing (oxidation) step (Correct Answer)
  • Mechanical retention through undercuts and beads on the coping only
  • A resin bonding agent applied between the metal and porcelain
  • Van der Waals forces between gold atoms and silica, with no oxide layer

Explanation

Metal-ceramic bonding involves several mechanisms: chemical bonding (the most important), mechanical interlocking (micro-roughness from airborne-particle abrasion), compressive forces (the metal's coefficient of thermal expansion is slightly higher than that of the porcelain, so the porcelain is placed under residual compression as it cools) and van der Waals forces. Chemical bonding needs a thin, adherent oxide layer on the metal surface. Gold, palladium and platinum do not oxidise readily, so high-noble and noble alloys contain small amounts of oxide-forming elements such as tin, indium, iron, gallium and zinc. During the degassing or oxidation firing, these diffuse to the surface and form oxides that dissolve into the opaque porcelain, creating a continuous transition. In base metal alloys (Ni-Cr, Co-Cr), chromium oxide is formed, but an overly thick oxide layer weakens the bond and causes failure within the oxide itself. The most common failure mode in a good bond is cohesive failure within the porcelain. Beryllium in some Ni-Cr alloys improves castability and bonding but is toxic. The metal coping design should support porcelain of uniform thickness (about 1-1.5 mm, no more than 2 mm) and avoid sharp angles.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs