In high-copper dental amalgam, the gamma-2 phase is eliminated mainly through formation of:

41 views
  • Cu3Sn (epsilon)
  • Ag2Hg3 (gamma-1)
  • Cu6Sn5 (eta) (Correct Answer)
  • Ag3Sn (gamma)

Explanation

In low-copper amalgam, the gamma phase (Ag3Sn) reacts with mercury to form gamma-1 (Ag2Hg3), which is the matrix, and gamma-2 (Sn7-8Hg), with unreacted gamma particles remaining as a filler. Gamma-2 is the weakest, softest and most corrosion-prone phase. Its corrosion releases mercury and tin products, and is linked to marginal breakdown, creep and loss of strength. In high-copper admixed alloys, gamma-2 initially forms but then reacts with silver-copper eutectic particles to form Cu6Sn5 (the eta-prime phase) plus gamma-1, so gamma-2 is essentially eliminated. In single-composition (unicompositional) high-copper alloys, Cu6Sn5 forms directly as rods within the gamma-1 matrix without a gamma-2 stage. Cu3Sn (epsilon) is present in the original alloy particles and is not the phase that replaces gamma-2. As a result, high-copper amalgams show better corrosion resistance, lower creep, higher early strength and better marginal integrity.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs