In high-copper dental amalgam, the gamma-2 phase is eliminated mainly by formation of:

45 views
  • Ag2Hg3 (gamma-1)
  • Ag3Sn (gamma)
  • Cu6Sn5 (eta-prime) (Correct Answer)
  • Cu3Sn (epsilon)

Explanation

In conventional low-copper amalgam, the setting reaction is gamma (Ag3Sn) + Hg -> gamma-1 (Ag2Hg3) + gamma-2 (Sn7-8Hg) + unreacted gamma. The gamma-2 phase is the weakest, softest and most corrosion-prone phase. Corrosion of gamma-2 releases tin and mercury, which causes creep, marginal breakdown ("ditching") and loss of strength. High-copper alloys (more than 12% copper) were developed to eliminate it. In admixed (dispersed-phase) alloys, silver-copper eutectic particles are added to the conventional lathe-cut particles. In a secondary reaction, the gamma-2 that forms initially reacts with the Ag-Cu particles to produce Cu6Sn5 (eta-prime) and more gamma-1. In single-composition (unicompositional) alloys, the ternary Ag-Sn-Cu particles react with mercury so that eta-prime forms directly, and gamma-2 does not form at all. Eta-prime crystals also interlock and help resist creep. As a result, high-copper amalgams have lower creep, greater early and final compressive strength, better corrosion resistance and much better long-term marginal integrity. The epsilon phase (Cu3Sn) is present in the alloy particles themselves and is not the product that replaces gamma-2.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs