In high-copper amalgams, the gamma-2 phase is eliminated because tin preferentially combines with copper to form:
- Cu6Sn5 (eta phase) (Correct Answer)
- Ag2Hg3 (gamma-1 phase)
- Cu3Sn (epsilon phase)
- Ag3Sn (gamma phase)
Explanation
In conventional low-copper amalgam, the setting reaction is: gamma (Ag3Sn) + Hg gives gamma-1 (Ag2Hg3) + gamma-2 (Sn7-8Hg) + unreacted gamma. The gamma-2 phase is the weakest, most corrodible phase. Its corrosion lowers strength, causes marginal breakdown and increases creep, and released mercury reacts with residual gamma particles causing mercuroscopic expansion. In high-copper alloys (copper content 12-30%), either admixed (with Ag-Cu eutectic spheres) or single-composition (Ag-Sn-Cu particles), tin preferentially reacts with copper to form the eta phase Cu6Sn5, so gamma-2 is eliminated or greatly reduced. For admixed alloy, there is a secondary reaction in which gamma-2 reacts with Ag-Cu particles to form eta plus gamma-1. Clinical advantages are higher early compressive strength, lower creep (often less than 0.1%), better corrosion resistance and improved marginal integrity, so high-copper alloys are now standard. The epsilon phase Cu3Sn is present in single-composition alloy particles. Zinc in the alloy acts as a deoxidizer but causes delayed expansion if contaminated by moisture during condensation.