In dental porcelain systems, which oxide is primarily responsible for the coefficient of thermal expansion matching required for successful metal-ceramic bonding?
25 views
- Potassium oxide (K₂O) (Correct Answer)
- Sodium oxide (Na₂O)
- Boron oxide (B₂O₃)
- Aluminum oxide (Al₂O₃)
Explanation
Potassium oxide (K₂O) controls CTE matching due to its large ionic radius disrupting silicon-oxygen networks, increasing thermal expansion. By adjusting K₂O content (8-12% for base metals, 4-8% for gold alloys), manufacturers match porcelain CTE to different alloys. Base metals require higher K₂O content for their higher CTEs (13.5-14.5×10⁻⁶/°C). Porcelain must have CTE 0.5-1.0×10⁻⁶/°C less than metal for residual compression.