In all-ceramic crown preparations (e.g., for lithium disilicate), the recommended minimum occlusal reduction is greater than for metal-ceramic crowns primarily because:

15 views
  • Ceramic is weaker in tension and requires greater bulk for strength (Correct Answer)
  • To provide space for aesthetic layering of porcelain
  • The bonding process requires additional space for the resin cement layer
  • To compensate for the higher thermal conductivity of ceramics

Explanation

All-ceramic materials, like lithium disilicate (e.g., IPS e.max), are brittle and susceptible to tensile failure (fracture) under loading. To withstand occlusal forces, they require adequate bulk (thickness) to distribute stresses and prevent flexural failure. The recommended minimum occlusal reduction is 1.5-2.0 mm for all-ceramic crowns, compared to 1.5 mm for metal-ceramic crowns (where the metal coping provides strength). This extra reduction ensures there is sufficient ceramic thickness for strength and durability, especially in areas of high stress like centric holding cusps. While aesthetics (B) is a factor, it's not the primary reason for minimum reduction—even monolithic (single-layer) ceramics need this bulk. Cement space (C) is minimal (~50-100 µm) and planned separately. Thermal conductivity (D) is not a major design factor. Inadequate reduction is a leading cause of all-ceramic crown fracture.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs