Gaseous porosity in the thickest region of a heat-cured acrylic denture base is mainly caused by:

34 views
  • Raising the temperature too rapidly so that monomer boils (Correct Answer)
  • Insufficient packing pressure
  • Excess polymer in the dough
  • Inadequate trial closure

Explanation

Gaseous porosity occurs in thick sections of the denture where the exothermic heat of polymerisation cannot dissipate. If the flask is heated too rapidly, the temperature inside the resin rises above the boiling point of methyl methacrylate monomer (100.8 degrees Celsius), and the monomer boils, producing small, uniform, spherical voids in the thickest portions, away from the surface. Prevention involves a slow curing cycle, for example 74 degrees Celsius for 8 or 9 hours, or 74 degrees for 2 hours followed by 100 degrees for 1 hour. In contrast, insufficient packing pressure or inadequate dough causes contraction porosity, which consists of irregular voids distributed throughout the denture, often near the surface.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs