Following is correct about setting time of product?
17 views
- incomplete calcination, faster the set
- increase w/p ratio, increase the setting time
- increase spatulation, decrease the setting time
- All of above (Correct Answer)
Explanation
If Excess gypsum (dihydrate) left in fina product, Resulting plaster set faster.
If Soluble anhydrite is in excess, faster will set,
If Natural anhydrite is In excess, slower will be the set
Finer (smaller) the particle size, faster will set