During the setting of zinc phosphate cement, the powder is incorporated into the liquid in small increments on a cooled glass slab. Which of the following best explains the primary rationale for this technique?
21 views
- To decrease the viscosity of the final mix
- To extend the working time by controlling the exothermic reaction (Correct Answer)
- To reduce the film thickness
- To increase the compressive strength
Explanation
Zinc phosphate cement setting is highly exothermic, releasing approximately 130°C if mixed rapidly. The reaction rate doubles for every 10°C increase (Arrhenius equation). By incorporating powder in small increments on a cooled glass slab (18-24°C), heat is dissipated effectively, extending working time from 2-3 minutes to 5-6 minutes while maintaining adequate setting time.