During the polymerization of denture base acrylic resin, which processing parameter MOST effectively reduces residual monomer levels to improve biocompatibility and physical properties?
27 views
- Increasing the powder/liquid ratio
- Extending the terminal boiling cycle duration
- Using a slow heat polymerization cycle with proper terminal heat treatment (Correct Answer)
- Applying higher clamping pressure during flask closure
Explanation
Slow-heat polymerization (74°C for 8-9 hours below MMA boiling point 100.3°C) followed by terminal heat treatment (100°C for 1-3 hours) most effectively reduces residual monomer (typically 0.2-5%). Terminal boiling mobilizes trapped monomer, allows continued polymerization of unreacted MMA, and increases degree of conversion. This reduces residual monomer to <0.5%, minimizing mucosal irritation, allergic reactions, and improving mechanical properties versus fast cycles.