During the fabrication of a cast metal partial denture framework, the casting exhibits surface nodules and roughness. Which defect in the investing and casting process is MOST likely responsible?

20 views
  • Investment setting expansion was too high
  • Rapid heating of the investment mold trapped gases
  • The burnout temperature was insufficient to eliminate wax residue
  • Investment broke down at high temperature, releasing gases (Correct Answer)

Explanation

Surface nodules result from investment thermal decomposition at extreme casting temperatures (1000-1400°C). Gypsum-bonded investments decompose above 700°C, releasing SO₂ and water vapor. At metal-investment interface, breakdown releases gases trapped as metal solidifies, creating surface irregularities and nodules. Distinct from internal porosity, this produces characteristic surface texture defects at the critical metal-mold interface.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs