Delayed expansion of an amalgam restoration, which may cause pain, protrusion of the restoration and fracture, occurs when:
- A zinc-containing alloy is contaminated with moisture during trituration or condensation, producing hydrogen gas (Correct Answer)
- The amalgam is condensed with excessive force
- A zinc-free alloy is over-triturated
- The restoration is polished within 24 hours
Explanation
Zinc is added to some amalgam alloys (up to about 1-2 percent) as a deoxidiser (scavenger) during alloy manufacture, because it combines with oxygen more readily than the other metals and thus prevents oxidation of silver, tin and copper; it also improves plasticity and may improve clinical longevity. However, if a zinc-containing low-copper or high-copper alloy is contaminated with moisture (saliva, blood or water from the hands) during trituration or condensation, the zinc reacts with water to form zinc oxide and hydrogen gas: Zn + H2O gives ZnO + H2. The hydrogen does not combine with the amalgam; it accumulates within the restoration, building up internal pressure, which causes the restoration to expand. This delayed (secondary) expansion usually begins 3-5 days after insertion and may continue for months, reaching values of more than 4 percent (400 micrometres per cm). Clinical consequences include pressure pain (because the expanding restoration presses on the pulp), protrusion of the restoration out of the cavity, increased microleakage, surface blistering, corrosion, and fracture of the restoration or the tooth. Prevention includes proper isolation, preferably with a rubber dam, and the use of zinc-free alloys when moisture control is difficult. Normal dimensional changes on setting, according to ADA specification No. 1, should be within plus or minus 20 micrometres per cm. Modern spherical, high-copper alloys mixed in capsules contract slightly during setting.