An addition silicone (polyvinyl siloxane) impression fails to set in areas that were touched by the assistant's gloved fingers during tray loading. The most likely cause is:
- Ethanol by-product released from the material
- Sulphur compounds from latex gloves poisoning the platinum catalyst (Correct Answer)
- Use of a custom tray that was too rigid
- Excess humidity accelerating the reaction
Explanation
Elastomeric impression materials include polysulphides, condensation silicones, addition silicones (polyvinyl siloxanes, PVS) and polyethers. Addition silicones set by an addition polymerisation reaction between vinyl-terminated polydimethylsiloxane and a silane (containing silicon-hydrogen bonds), catalysed by a platinum salt (chloroplatinic acid). Because no by-product is formed (unless hydrogen gas is released through a side reaction with residual silane or moisture), PVS has the best dimensional stability of all impression materials, allowing multiple pours and delayed pouring (up to 1-2 weeks), but if hydrogen is released, pouring should be delayed by about 1 hour or palladium can be added as a hydrogen absorber. The platinum catalyst is inhibited ("poisoned") by sulphur compounds, which are present in latex gloves (from dithiocarbamates used in vulcanisation) and in some retraction cords containing ferric sulphate or aluminium sulphate, and by residual monomer of some acrylic resins and methacrylate-based materials. Touching the putty or the prepared teeth with latex gloves can prevent or retard polymerisation in those areas, producing a sticky, unset surface and an inaccurate impression. Vinyl or nitrile gloves should be used, and the teeth should be cleaned of any contaminants. Condensation silicones release ethanol as a by-product, causing shrinkage and poor dimensional stability, so they must be poured immediately; polysulphides release water. Polyethers are stiff, hydrophilic and absorb water, so they should not be stored in humid conditions.