A monolithic zirconia crown is to be cemented with a resin cement. Unlike lithium disilicate, zirconia cannot be effectively etched with hydrofluoric acid. The recommended surface treatment for zirconia is:

34 views
  • 37% phosphoric acid for 60 seconds followed by an unfilled resin
  • Airborne-particle abrasion with alumina at low pressure followed by an MDP-containing primer (Correct Answer)
  • Coating with a thin layer of feldspathic porcelain before cementation
  • 5% hydrofluoric acid for 20 seconds followed by a silane coupling agent

Explanation

Glass-ceramics such as feldspathic porcelain, leucite-reinforced ceramic and lithium disilicate contain a silica-based glassy phase. Hydrofluoric acid (usually 5% for 20 seconds for lithium disilicate) dissolves this phase selectively to create micromechanical retention, and silane then provides a chemical link between the silica and the methacrylate resin. Zirconia (yttria-stabilised tetragonal zirconia polycrystal, Y-TZP) is a polycrystalline oxide ceramic with no glassy phase, so it is acid-resistant and cannot be etched or silanated effectively. The evidence-based APC concept (Blatz) for bonding to zirconia is: A, airborne-particle abrasion with 50 micrometre alumina at low pressure (about 1-2 bar) to clean and roughen the surface; P, a primer containing 10-MDP (10-methacryloyloxydecyl dihydrogen phosphate), whose phosphate group forms a chemical bond with zirconium oxide; C, a composite resin cement, ideally a dual-cure cement. Airborne-particle abrasion may cause a small amount of tetragonal-to-monoclinic phase transformation. Contamination with saliva after try-in must be removed, for example with a zirconium oxide cleaning paste such as Ivoclean. Conventional cementation with glass ionomer is acceptable when the preparation provides good retention.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs