A maxillary complete denture fabricated with heat-polymerized acrylic resin exhibits midline fracture after 18 months of service. Which factor in the denture processing technique MOST significantly contributed to this failure?

25 views
  • Insufficient thickness of acrylic resin at the midline
  • Inadequate curing time during polymerization
  • Deflection of the denture during flask closure creating internal stress (Correct Answer)
  • Using a fast polymerization cycle instead of slow cycle

Explanation

Midline fractures result from residual internal stresses from flask closure deflection. When teeth position or packing pressure causes cast deflection, acrylic polymerizes in stressed state with "locked-in" stresses. During function, flexural forces (concentrated at midline due to absent tissue support) plus cyclic loading eventually exceed residual strength, causing fatigue failure typically at 12-24 months. This explains delayed fracture versus immediate failure.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs