A dental laboratory technician observes that a phosphate-bonded investment mold for casting a Ni-Cr partial denture framework shows surface cracking after burnout. What is the PRIMARY cause of this defect?

31 views
  • Too rapid heating rate during burnout (Correct Answer)
  • Insufficient water used during mixing
  • Investment was allowed to set for too long before investing the pattern
  • Burnout temperature exceeded the thermal stability limit of the investment

Explanation

Rapid heating causes thermal shock cracking in phosphate-bonded investments. Critical phase transformations (water evaporation at 100°C, binder decomposition at 200-400°C, quartz inversion at 573°C with 2-3% volume change) create stress gradients when heating exceeds 10-15°C/minute. Surface heats faster than interior, creating tensile stresses exceeding investment strength. Proper burnout requires controlled heating: 60 minutes to 300°C, hold 30-60 minutes, then 60-90 minutes to 900-950°C.

Comments (0)

No comments yet. Be the first to comment!

Want to practice more?

Explore thousands of MCQs across every exam category on Exams Nepal.

Find More MCQs