A Class II MO composite restoration on a molar is 4 mm deep at the gingival seat and the cavity has a C-factor of ~2. You are using a conventional methacrylate-based composite (polymerization shrinkage 2.5%) and an adhesive system that produces an average dentin bond strength of 20 MPa. Which strategy most effectively minimizes cuspal deflection and marginal gap formation during light curing?
- Use incremental oblique filling (2 mm increments) + high-intensity continuous curing (1200 mW/cm² for 20 s)
- Use a single bulk fill (4 mm) low-shrinkage composite + soft-start curing (ramped from 200 to 1200 mW/cm²)
- Use 2 mm increments and apply a pre-polymerization low-irradiance (soft-start) pulse for 5 s followed by 20 s high intensity for each increment (Correct Answer)
- Use bulk fill + immediate post-cure light press to seat restoration and overcome shrinkage
Explanation
Minimizing polymerization shrinkage stresses in a moderate-to-high C-factor cavity requires reducing the rate of polymerization so stress can be relieved by flow before gelation (soft-start), combined with incremental placement to reduce overall shrinkage strain per increment and to change stress vectors. Option C applies both incremental technique and soft-start partial cure (pre-polymerization low irradiance) then full cure — this balances degree of conversion with stress relaxation. Option A (high-intensity continuous) accelerates gelation and increases stress. Option B bulk fill may reduce handling time but not necessarily minimize stress unless the material has demonstrated low shrinkage stress; still bulk fill + soft-start could be reasonable but C is superior because of incremental control. Option D (pressing after bulk polymerization) cannot overcome tensile interfacial stresses and risks further disrupting the adhesive interface.